This section consists of Reheat furnace which reheat the steel sections coming from the CCM up to 1200 C then send it to be rolled in the rolling line which contain 8 stages. This process makes sure that the produced bars meet the required standard without any malformation. The final product then carried out to a cooling bed and using a special movement this movement generates an air swirl which cools the bars slowly preventing sudden temperature drops in the final products.

2-مرحلة-الدرفلة-1024x768

ROLLING STAGE

Finally packing machine used to pack the reinforcements bars in packs of 2 tons each.

-الدرفلة-1024x768

ROLLING PHASE

-الرزم-1024x768

PACKET PHASE

-التبريد-1024x768

COOLING LINE

-الوسطي-1024x768

MIDDLE OVEN